FFKM High-Temp 75P grade card: FFKM-HT75P-01, design range −15 to 300 °C.
Pascalor
Technical data sheet
Engineered for extremes

FFKM High-Temp 75P

FFKM-HT75P-01

Read the code: FFKM, HT duty (high temperature), 75 Shore A, P for peroxide cure, recipe 01.

Development grade. The values below are design targets, not measured results. Each target becomes a typical value, with the number of lots and the test report behind it, as testing is completed.

A 75 Shore A FFKM for the highest temperatures and the broadest chemistry: steam and hot water, acids, bases, amines and aromatics; to 300 °C in dry heat, with a steam limit to be set from test data (target 250 °C).

Polymer class
FFKM
Duty
HT: high temperature
Pole mark
HPHT
Hardness
75 Shore A
Temperature range
-15 to 300 °C
Lead time
Trial quantities on request
Minimum order
25 kg
Issued
2026-10-28
Revision
A
Packing
Per order

Design targets and release limits

PropertyTargetLimitsUnitMethod
Hardness7570 to 80Shore AASTM D2240 / ISO 48-4, 1 s
Specific gravity2±0.03 of approved valueASTM D297 / ISO 2781
Tensile strength15min 12MPaASTM D412 die C / ISO 37 type 2
Elongation at break170min 130%ASTM D412 die C / ISO 37 type 2
Modulus at 100 %75 to 9MPaASTM D412 die C / ISO 37 type 2
Compression set, 70 h at 250 °C25max 35%ASTM D395 method B, button
TR10-2max 0°CASTM D1329 / ISO 2921
Saturated steam, 168 h at 250 °C, volume change+3max 6%In-house autoclave method
Heat ageing 70 h at 300 °C, hardness change+30 to 6pointsASTM D573 / ISO 188

Qualification plan

The grade code says what this compound is designed for. This table says what it has passed: a duty is claimed only once its report is on file.

TestStandard or methodConditionsStatus
Steam ageingIn-house autoclave method, published with results168 h and 500 h at 250 °CPlanned
Long-term heat ageingASTM D573 / ISO 1881,000 h at 300 °CPlanned
Sour ageing and life predictionISO 23936-2 Annex A / NORSOK M-710Sour multiphase fluid (hydrocarbon liquid, water, gas with H2S) at three temperatures; Arrhenius extrapolation to service temperaturePlanned
Mechanical seal approvalPump OEM qualification (API 682 seals)Per OEMPlanned

Design targets are the values the compound is designed to reach. They are not measured results and they are not a warranty. Release limits apply to lots once the recipe is approved. The grade code says what the compound is designed for; the qualification plan says what it has passed. Confirm suitability in your own application and fluids.

Every lot is supplied with a certificate of analysis. Enter the lot ID under Track on the website to see the lot record. Pascalor is an independent brand and is not affiliated with any polymer manufacturer named elsewhere on this site.