Low-temperature FKM: the options and what to ask a supplier

Standard FKM stiffens in the cold. Here is how low-temperature FKM is built, what the cold-end numbers mean, and the questions that reveal whether a grade will seal when it matters.

Intermediate2 min readBlogUpdated 2026-10-24FKMFEPMHNBR
Cover image: "Low-temperature FKM: the options and what to ask a supplier", with a cold snowflake disc.

A general-purpose FKM is chosen for heat and chemicals. Its weak point is the cold. For cold-climate pipelines, LNG-adjacent equipment and winter start-up, the question becomes: which compound still seals at the low end of the window?

Why FKM stiffens

The glass transition temperature (Tg) of a rubber marks where it changes from rubbery to stiff. A typical general-purpose FKM has a Tg a little below -15 °C. Seals begin to lose useful recovery near that point, so the practical sealing limit sits a few degrees above it, often around -20 °C. Chemistry changes (more flexible monomers, different fluorine content, special polymer types) move Tg lower, at a price in fluid resistance or cost.

The approaches in plain terms

  • Low-temperature FKM types built from different monomers, giving a lower Tg while keeping much of the heat and fluid resistance.
  • Blends and compounding choices such as plasticiser type. Take care: a plasticiser that helps in the cold can extract in service.
  • A different polymer when the fluid allows it. HNBR with lower acrylonitrile content is more flexible in the cold. Ask about its limits in sour or amine service.

What the cold-end numbers mean

  • Tg by DSC tells you where the transition sits. It is not the sealing limit.
  • TR10 (ASTM D1329) is the temperature at which a stretched, frozen sample has retracted by 10 percent. It is closer to the practical limit.
  • Compression set at low temperature (ASTM D1299 or ISO 815-2) shows whether a seal springs back after being held cold.
  • Brittleness temperature (ASTM D2137) is a failure limit, not a sealing limit.

Questions to ask

  1. Which low-temperature test, at which temperature, and what was the result?
  2. Is compression set reported after both heat ageing and cold holding?
  3. What is the effect on fluid swelling and heat ageing compared with a standard grade?
  4. Does the lot record report the same tests, so you can see consistency?

Our LT and ULT grades are written for this duty. FKM Low-Temp 90P (FKM-LT90P-01) and FKM Ultra-Low-Temp 90P (FKM-ULT90P-01) on the compounds page show how the targets, limits and test plan are laid out. State your own cold and hot ends and we will propose candidates.

About this article. It is original writing prepared from public sources, standards and general industry practice. It is not a copy of any book or standard and it is not engineering advice. Confirm values against the current edition of the standard and test in your own application. Only analyse material you own or are entitled to analyse.